Titanium-based superalloy powder titanium alloy powder for 3

Titanium-based superalloy powder for 3D printing

 

category

Alloy grades and characteristics

Alloy number:

TA0,TA1,TC4,TC4 ELI,TC11,TC17,TC18,TC21,TA7,TA12,TA15,TA17,TA19,Ti40,Ti60,TiAl(Ti36Al,Ti48Al2Cr2Nb),TiNi,TiNb,ZrTi

Particle size:

0-20μm, 15-45μm, 15-53μm, 53-105μm, 53-150μm, 105-250μm

Morphology:

Spherical or nearly spherical

Appearance:

Grey

Package:

Aluminum bag,Vacuum packing

Application:

3D printing metal powder

Other applications:

powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.

 